Anti-aliasing and exposure are the two slicer dials that most directly determine whether your resin prints measure like the CAD model—especially edges and holes. If your part is consistently too large, too small, or your holes never land on size, it’s rarely a single setting.
This guide gives you a practical, end-to-end method to tune AA and exposure using a printed test geometry, calipers, and a simple measurement loop. The goal is dimensional accuracy in XY and predictable hole fit, not just a nicer-looking surface.
Understand Anti-AAliasing and Exposure in Resin Printing

Anti-aliasing (AA) changes how the slicer blends the pixels for sloped curves and angled edges. In practice, that can:
- Smooth stepped “jaggies” on circles and diagonals
- Alter where the software decides an edge starts and ends
- Impact both outer dimensions (like a block edge) and inner features (like hole diameters), sometimes in different ways
Exposure time (and the related light settings like initial exposure and delays) controls how far the cured area spreads within and beyond a pixel. If exposure is too high, features can “grow” and holes can constrict. If exposure is too low, features can “shrink” and holes can become larger than intended.
The key idea: AA and exposure are not interchangeable.
- AA is primarily about edge shaping and pixel blending.
- Exposure is primarily about cure strength and penetration.
For dimensional accuracy, you’ll get the most reliable results if you separate the tuning process: lock exposure first (with AA held constant or minimized), then tune AA for edge quality while preserving size.
Print Test Geometry for XY Edges and Hole Accuracy

A good resin accuracy test geometry is typically a flat plate with:
- Outer squares or rectangles with known side lengths
- A stepped wall or stepped gauge block (to see how curved/angled edges respond)
- Multiple through-holes or blind holes with known diameters
- At least one set of holes close together (so you can check center-to-center spacing)
Why this matters: outer dimensions tell you whether your XY scale is off; hole diameters tell you how concave surfaces behave under the cure process. Center-to-center spacing helps you catch “stretch” or scaling issues separately from hole shrink/constriction.
Before printing the test part, keep everything else consistent so you’re not chasing noise:
- Use the same resin and temperature (resin viscosity affects flow and curing behavior)
- Level the build plate and verify vat cleanliness
- Use the same layer height and the same orientation as your real prints
- Stir/condition resin so it’s not settling into a different concentration
Measure With Calipers and Record the Metrics
After post-curing (including the same wash and post-cure process you normally use), measure the test part while it’s stable and fully cured.
You’re looking for repeatable, directionally consistent errors—not random variation. Measure at the same locations each time:
- Outer edge length: measure along multiple sides if present (e.g., all four edges of a square)
- Hole diameter: measure near the opening and again deeper if the hole is blind; for through-holes, measure across the clear opening
- Hole spacing: measure center-to-center for at least one pair of holes
Write down three categories of results:
- Outer size error (measured minus nominal)
- Hole diameter error (measured minus nominal)
- Spacing error (measured minus nominal)
A helpful interpretation guide:
- If all XY sizes are uniformly off (outer edges and spacing), you likely have a more global XY scale/cure strength issue.
- If outer dimensions look close but holes are consistently wrong, AA and/or how concave surfaces cure is the bigger factor.
- If holes close up (measured diameter smaller than nominal), exposure is often too strong, or AA is pushing edges inward.
- If holes open up (measured diameter larger than nominal), exposure may be too weak, or AA may be under-blending edges.
Tune Exposure First, Then Anti-Aliasing for Size-Preserving Edges
To avoid mixing effects, use a two-phase tuning approach.
Phase 1: Exposure tuning (AA minimized or held constant)
- Start with AA set to your slicer’s lowest level or a consistent baseline you’re not afraid to change later.
- Adjust exposure in small, deliberate steps.
- Print the same test geometry.
- Compare measured outer dimensions and hole diameters against nominal.
If your prints are too big (outer dimensions too large, holes too small), reduce exposure.
If your prints are too small (outer dimensions too small, holes too large), increase exposure.
Phase 2: AA tuning (exposure held constant)
- Once exposure is close enough that outer sizes and hole diameters are in the right direction (not wildly off), stop touching exposure.
- Now change AA level to improve edge quality while keeping size steady.
- Print the test geometry again and re-measure.
What to expect as you raise or lower AA:
- Higher AA often improves the visual roundness of curves and diagonals, but it can also shift effective edge placement.
- You may see holes react differently than outer walls. That’s normal—concave edges can blend differently under the AA algorithm.
The target isn’t “best-looking AA.” The target is: edges and holes that land on size with acceptable tolerance.
Use a Simple Measurement Loop to Lock In Your Settings
You don’t need a spreadsheet-heavy workflow to get consistent results. Use this tight loop, and change only one variable at a time.
- Pick a baseline: choose your current AA setting and start with an exposure you’re confident is not completely out of family for your resin.
- Print test geometry #1 using that baseline.
- Post-cure the part exactly like your real jobs, then measure outer edges, hole diameters, and center-to-center spacing with calipers.
- Decide which “error direction” you have: too large XY/too small holes means reduce exposure; too small XY/too large holes means increase exposure.
- Adjust exposure only (AA unchanged) by a small step and print test geometry #2.
- Repeat until outer dimensions and hole diameters are both close to nominal in the same sense you want (for example, outer within tolerance and holes no longer consistently closed-up).
- Once exposure is tuned, keep exposure fixed and adjust AA in smaller steps. After each AA change, print the test geometry and re-measure holes and edges. Stop when AA improves edge smoothness without breaking hole fit.
This loop works because it forces a cause-and-effect relationship:
- During Phase 1, exposure changes are the only cure-strength change.
- During Phase 2, AA changes are the only edge-blending change.
If you find yourself stuck (for example, exposure changes help outer dimensions but hole diameters swing wildly), consider two practical checks before doing another round of tuning:
- Confirm your wash and post-cure process is consistent. Over-curing can make surfaces harden in a way that changes apparent hole opening.
- Make sure your measurement method is consistent. Resin holes can have slightly different profiles at the entrance versus deeper down.
Once your settings are stable, you can refine with “one last tweak” rather than constant iteration. For example, if holes are consistently a touch small but outer edges are already close, that’s usually where AA or a targeted hole compensation (if your slicer offers it) can help—without re-opening the entire exposure calibration.
Finally, when you move from test parts to real models:
- Keep the same layer height and orientation.
- Re-check the specific critical feature (often one key hole size) first.
- Expect that very small features and very large features may not behave identically; use the test part to bracket what “accurate” means for your printer and resin.
PriceIt3D may earn a commission when you buy through links on this page, at no extra cost to you. Affiliate notice.